化合物材料
chemical materials
利用我们超过80年的在纤维素制备上的成熟技术,旭化成(Asahi Kasei)发 明了拥有专利的彩色纳米微球。当在侧向流层析免疫检测中使用该纳米微球, 不仅能提高反应灵敏度,缩短检测时间,纤维素的独特特性亦能带来多种颜色 的选择。
侧向流免疫检测标记物革命
使用实例
NanoAct 与胶体金相比,它具有极好的可见度
在夹心法及竞争法测定中,使用NanoAct的试剂性能均优于胶体金。
产品信息
Cat# | Type | Color |
Diameter(nm) |
OD(ABS,1wt9) | Conc,(wt9) |
RE1AA |
Passive Adsorption |
Red | 330 | 225 | 1.0 |
RE2AA | Dark Red | 340 | 240 | ||
BL1AA | Navy | 325 | 250 | ||
BL2AA | Dark Navy | 365 | 265 | ||
GR1AA | Green | 335 | 160 | ||
KR1AA | Black | 350 | 150 | ||
RE1CA |
Covalent (COOH) |
Red | 335 | 220 | |
BL1CA | Navy | 320 | 230 | ||
GR1CA | Green | 335 | 155 |
◆ 荧光微球根据客户需要,即将上市。
◆ 除了标准型号,旭化成可根据客户需要提供定制粒径,颜色,OD值的微球产品。
1. 样品垫
· 高流速
· 极低的纤维析出
· 无黏合剂
· PET制作的样品垫有三层结构,中间层的超细纤维起过滤作用。
2. 结合垫
· 极低的纤维析出
3. 吸收垫
·PET超细纤维经过亲水处理
·均一性以及快速的吸水锁水性
· 无黏合剂
产品信息
Cat# |
Reference (Old Item#) |
Application |
Material Composition |
Basis Weight (g/m²) |
Thick ness (mm) |
Wicking Rate (sec/4cm) |
CBSP060 | S-01 | Sample pad | Cupro (Cellulose) |
60 | 0.47 | 23 |
CBSP100 | S-02 | 100 | 0.39 | 13 | ||
CBSP097 | S-06 | Cupro/PE/PET | 97 | 0.34 | 26 | |
PPSP100 | A-01 | PET(Three layer/SMS) | 100 | 0.25 | 115 | |
PMAP080 | AK2-1 |
Sample pad/ Absorbent pad |
PET (Microfiber) |
80 | 0.19 | 67 |
PMAP090 | AK2-2 | 90 | 0.38 | 28 | ||
PSCP250 | 250Y | Conjugate pad | PET Coarse FIBER | 250 | 0.54 | - |
◆ 可根据客户要求,定制规格和形状
Cat# |
Water Absorbent |
Features | Refered Material |
CBSP060 | hydrophilic |
◆ Fast liquid retention and spreading ◆ High purity |
Cellulose nonwoven. |
CBSP100 | |||
CBSP097 | |||
PPSP100 | hydrophobic | ◆ Microfiberin the middle layer expected toworkas filte | |
PMAP080 |
hydrophilic treatment |
◆ Uniformity ◆ Very fast liquid retention and absorbency |
|
PMAP090 | |||
PMAP180 | Celulose nonwoven,paper high basis weight(+200g/m²) | ||
PSCP250 | hydrophobic |
◆ Uniformity ◆ Less hazardous in process |
Grass fibe |
横向流动分析开发服务
Our Lateral Flowlmmunoassay Development Service | ||
ltem | Feasibility Study | Project |
Service outline | Development service based on feasibility study request form | Onerous development service based on Contract developmentagreement |
Fee for Service | Free up to 7 days | Charge for the man-hours and reagents |
Delivery Period | Min.7days | Discussedin contract |
Fee for NanoAct | Free | Free |
Payment term | - | After receiving deliverables |
Deliverables | Verbal orbrief written report | Written report with all information |
Application Process | Feasibility study request form | Contract developmentagreement |
◆ 费用及交付周期将依据您的要求和计划。
◆ 我们可根据您的要求提供样品。
◆ 请根据下列联系方式咨询或提出您的要求。